    #46
    Re: Replasticizing hop balls

    Merl - how are your hop balls doing? I tried ATBC in a Benny Bull by Waliki. It had imperfections in the vinyl that can’t be seen from the outside. One day a weak spot let go. I was watching tv and heard psssssss. A one inch split developed and it is a strange material that won’t hold a repair. The Rody horse vinyl behaves like a hop ball so easier to repair a puncture/hole

    Comment

    • Guest

      #47
      Re: Replasticizing hop balls

      Experiment is done. Whatever was going to stretch has stretched, at least as much as I'm willing to push them. Unfortunate that the no name 1960s hopper wouldn't hold the tear aid but it's a lesson learned--it was just too cheaply molded to hold up to the ATBC. Sun Hoppity Hop responded best...Great Space Hopper is a solid but almost fibrous formulation that plasticizer got barely past where I'd already heat stretched it. Haven't paid attention to the Hop 66 even though it's dosed. I have no interest in doing anything with current cheap hoppers since they're already very rubbery, and not in a good way.

      Comment

      • Guest

        #48
        Re: Replasticizing hop balls

        Just got a late 1970s Romper jump ball, never used. Box says 13" diameter max...useless size...unless it could be stretched. It's now up to 16.25" and 17" high at the seat from only hot water stretching. Too bad it's so small...the vinyl is an excellent cross between the heavier stiffness and bounce of HH/SH and the floppy rubberiness of modern hoppers.

        Comment

        • Guest

          #49
          Re: Replasticizing hop balls

          If you're interested in trying this, ATBC does work but keep these things in mind.

          1. With old balls, ATBC gives good results when it works. It adds pliability to increased size where (in my experience) heat stretching alone adds size but reduces flexibility.

          2. The heavier and stiffer the old vinyl is, as formulations varied, the generally safer ATBC will be when the ball is put under pressure. With thinner, rubberier vinyl the effect can be unpredictable.

          3. Most importantly, ATBC exploits weaknesses that heat stretching alone doesn't seem to. If a used ball has ANY degree of normal damage beyond the barest surface scuffs (like moderare scratches or gouges that are otherwise fine, or visibly thinner spots from molding) the plasticizer WILL weaken these areas to the point of eventual failure. It has done this on four different balls I've dosed, and otherwise negligible damage or thin spots is what all had in common...and none popped while bouncing, they all blew spontaneously while just sitting there inflated because the weak spots were eaten through.

          My conclusion: only a ball that is consistently thick and undamaged, or in mint condition, should be replasticized with ATBC and stretched. Otherwise, you're better off relying on heat stretching.

          Good luck!
          Last edited by Guest; 25-11-2021, 14:15.

          Comment

          • Guest

            #50
            Re: Replasticizing hop balls

            Got a mint in box 1980s Hoppity Hop, never used, in the mail the other day. Immediately I added the plasticizer inside and out without fear of weakening pinholes or gouges that blew up the other ones I've experimented on.

            It is so "new" that the vinyl was very stiff and the ball got quite tight at only 15". I left it undisturbed for a full day. Measured it again tonight--it had expanded on its own (which it might have done anyway without ATBC) to almost 18 inches with some flex, so I warmed it under the shower and topped it off to 19 inches. 20" you may recall is the factory max. I'll leave it sit a few days to see if there's any more spontaneous stretch and go from there.

            Also found a mint 26" hopper from 2005, another unusual one but very well designed. Will post about that separately.
            Last edited by Guest; 10-02-2022, 00:05.

            Comment

            • Guest

              #51
              Re: Replasticizing hop balls

              Stretched 1/2 inch on its own since yesterday.

              Comment

              • Guest

                #52
                Re: Replasticizing hop balls

                20.1"

                Comment

                • Guest

                  #53
                  Re: Replasticizing hop balls

                  Do you have any pictures of the 2005 hopper? How big do you think the 1980s hoppity hop will go? I’m guessing 22”

                  Comment

                  • Guest

                    #54
                    Re: Replasticizing hop balls

                    The HH split near the bottom and blew out. Molding flaw I guess, as it barely got above rated. Biggest I ever got an HH is upthread, 23" was about as large as they'll go and still be usable. So that's it, I'm done stretching vintage.

                    Will post a photo of the new one this weekend.

                    How's the buoy?
                    Last edited by Guest; 17-02-2022, 21:49.