PVC PHR Level

Collapse
X
 
  • Time
  • Show
Clear All
new posts
  • Big Thud Joe
    Senior Member
    • May 2017
    • 407

    PVC PHR Level

    I know one of the participants told me on here that the ideal PHR level for PVC fetish use was about 65 to 70. This means I would have to get new sheeting made to spec. I know Gary from PVC U Like has the specified PVC.

    Dealing with his suggested factory in China, BeiLe Inflatables; Cheery notes that he's got material of 52-54 PHR on hand, so no new sheeting is required. This is for gloss white PVC and will be used for an inflatable noodle kind of cylinder shape.

    Can anyone advise me if this is still very soft, or more to the harder standards of today's crappy inflatables. Not doubting Gary's materials, just want to look into some other options, and if the difference between 50-54 verses 65-70 is negligible, then I'm hoping to try a sample of Cheery's 50-54 PHR stock.

    I'm not a sitter, nor a popper. I just like inflating my toys hard, then claw / dig my fingers in as I hug them. Absolute arousal starter is when I feel the PVC stretch when poking my fingers. I'll be suggesting DINP as the plasticizer.
  • PVC Vinyl Enthusiast
    PVC Fetish
    • Jan 2013
    • 197

    #2
    Originally posted by Big Thud Joe
    I know one of the participants told me on here that the ideal PHR level for PVC fetish use was about 65 to 70. This means I would have to get new sheeting made to spec. I know Gary from PVC U Like has the specified PVC.

    Dealing with his suggested factory in China, BeiLe Inflatables; Cheery notes that he's got material of 52-54 PHR on hand, so no new sheeting is required. This is for gloss white PVC and will be used for an inflatable noodle kind of cylinder shape.

    Can anyone advise me if this is still very soft, or more to the harder standards of today's crappy inflatables. Not doubting Gary's materials, just want to look into some other options, and if the difference between 50-54 verses 65-70 is negligible, then I'm hoping to try a sample of Cheery's 50-54 PHR stock.

    I'm not a sitter, nor a popper. I just like inflating my toys hard, then claw / dig my fingers in as I hug them. Absolute arousal starter is when I feel the PVC stretch when poking my fingers. I'll be suggesting DINP as the plasticizer.
    I concur that the 6P-free PVC used in many contemporary inflatables is very disappointing, in the sense that it lacks the same degree of softness, rubberiness, rustling and squeaking noise, the strong 'new PVC aroma' and 'stickiness' of the inflatables of the 1990s-early 2000s. I'd be pleased if the non-phthalate plasticizers gave the same result, but they don't.

    I've enclosed a short video clip of a 1990s-era inflatable chair I recently acquired; the soft, rubbery, 'sticky' and 'noisy' PVC material 'ticks all the boxes'!

    There is no reason why the China factories can't continue with the '1990s PVC formula' in contemporary inflatables, as there is no legislation forbidding the use of High Molecular Weight phthalate plasticizers like DINP (as a precautionary measure, the EU forbids use of DINP in babycare items, such as pacificers and small toys that can fit inside the mouths of babies and toddlers).

    Now to your query: I'd guess that the difference between 50-something PHR and 60-something/70-something PHR is quite discernible, but other factors also influence the perceived softness. One such factor is the Thickness of the PVC material. So, while 50-something PHR is a lower softness value than 60/70-something PHR, if the PVC film is thinner, it might feel quite soft even with a 50-something PHR.




    Enjoy soft, shiny and smooth PVC (inflatables and clothing). The 6P-free/10P-free material is total rubbish.